I ve seen j b weld break fail under certain circumstances but if you applied the product correctly and you re not expecting it to do something entirely unreasonable it s amazing stuff and i highly recommend it.
Jb weld kwik steel review.
After mixing it forms a permanent bond and can be shaped tapped filed sanded and drilled after curing.
If you re welding steel which is what most bikes are made of then it will be as strong as steel.
Read honest and unbiased product reviews from our users.
J b weld only adheres to the surface so the bond strength is actually only 1800 psi.
Once dried and cured it only can be removed by exposure to heat above 600 degrees fahrenheit sanding or filing off from the places it was applied.
A jb weld review shows that it can withstand temperatures up to 500 degrees fahrenheit.
Read honest and unbiased product reviews from our users.
Kwikweld is a fast setting version of the original j b weld two part epoxy cold weld system that provides strong lasting repairs to metal and multiple other surface types.
However they are both strong enough for most projects and repairs.
Kwikweld is a great alternative to original j b weld when you need a quick setting epoxy.
J b weld has a tensile strength of 3900 psi.
J b weld kwikweld is steel reinforced has a tensile strength of 3127 psi and can withstand temperatures up to 230 degrees fahrenheit 110 degrees celsius.
Because it is faster setting kwikweld has about two thirds the strength of j b weld.
A proper weld is as strong as the base material sometimes stronger.
When fully cured kwikweld is waterproof and resistant to petroleum chemical and acid.